CGM high-strength, non-shrink grout features early strength, high strength, high fluidity, and micro-expansion. It is widely used for secondary grouting of equipment foundations, anchoring of steel structure column bases, and the reinforcement or retrofitting of concrete structures.

Early and High Strength: Compressive strength reaches 30–50 MPa within 1–3 days. Bolts can be tightened or machinery test-run just 24 hours after application, while the 28-day compressive strength can exceed 60–90 MPa.
High Self-Flowing Capability: The grout self-levels and fills all voids under its own weight, eliminating the need for mechanical vibration.
Micro-Expansion: It does not shrink during hardening, ensuring tight contact between the equipment base, anchor bolts, and the foundation.
Durability and Impermeability: As an inorganic cementitious material, it resists oil penetration and high-temperature thermal shock, offering a service life superior to that of the base concrete.